Investment casting (also called precision or lost-wax casting) starts with a wax pattern made in a die. The pattern is coated layer by layer in a ceramic shell, the wax is melted out, and molten metal is poured into the cavity left behind. Parts come out close to final shape, with fine surfaces and consistent dimensions; complex shapes and thin walls that are difficult in sand casting become practical, and less machining is needed afterwards.
Our own valve bodies are made this way. Beyond valves, we take on investment castings to customer drawings: production is carried out by our partner factories, while Valand handles drawing and specification review, samples, production follow-up, inspection documents and export.
How investment casting works
- 1
Tooling
A wax-pattern die is made to your drawing.
- 2
Wax patterns
Wax patterns are injected and assembled onto a runner tree.
- 3
Shell building
Repeated dipping, stuccoing and drying build up the ceramic shell.
- 4
Dewax and firing
The wax is melted out and the shell is fired.
- 5
Pouring
Metal is melted to the specified grade and poured.
- 6
Finishing
Shell removal, gate cutting, grinding and heat treatment where required.
- 7
Machining and surface
CNC machining, polishing, pickling and passivation as required.
- 8
Inspection and shipment
Inspected to the agreed items, documented and shipped.
Materials available on request
| Material group | Typical grades | Properties and typical uses |
|---|---|---|
| Austenitic stainless steel | 304, 316, 316L (cast equivalents CF8, CF8M, CF3M) | Good corrosion resistance; valves, pumps, food and chemical equipment, marine hardware. |
| Martensitic stainless steel | 410, 420, 431 | Can be hardened by heat treatment; wear parts, valve trim, machine parts. |
| Precipitation-hardening stainless | 17-4PH (630) | High strength with corrosion resistance; load-bearing precision parts. |
| Carbon steel | 1020, 1045 and similar | Easy to machine and economical; structural and general machine parts. |
| Low-alloy steel | SCM415, SCM440 (4140 family) and similar | Heat-treatable for strength and toughness; automotive and machinery parts. |
| Nickel-based alloys | Inconel 625, 718 | Heat and corrosion resistant; high-temperature or severe service. Assessed case by case. |
The table lists common choices; it is not exhaustive, and not every grade suits every part. Feasibility, the material standard applied (for example ASTM, JIS or EN) and mechanical properties are confirmed after drawing review and stated in the quotation.
Typical parts
Samples and lead time
- A new part starts with tooling and samples; mass production follows sample approval.
- Production lead time depends on part complexity, quantity, heat treatment and secondary operations; a schedule is given with the quotation.
- Tooling cost and ownership are set out in the quotation.
- Your drawings are used only for quoting and production; a non-disclosure agreement can be arranged on request.
What to send for a casting enquiry
- Drawings: 2D with dimensions and tolerances, ideally a 3D file (STEP / IGES)
- Material grade and standard
- Batch quantity and estimated annual volume
- Part weight or overall size
- Heat treatment and hardness
- Machining and surface finish
- Inspection and documents required (e.g. material certificate, dimensional report)
- Required delivery time and destination port
Tell us your specification
We welcome enquiries from equipment builders, engineering contractors and distributors.